PPR Pipes laying can be divided into the installation of equipment, dark equipment laying, overhead laying and laying and other laying methods. As the PPR Pipes by the environment and the impact of medium temperature changes, it is appropriate to use the dark, the construction should be with the construction, structure, electrical and other professional closely with each other, coordinate each other, do a good job reservation, burial work, and take appropriate protection Measures. The wall should be reserved for the pipeline, the pipeline laying a good pressure should be filled around the tube at least 20mm thick rock wool and other soft materials to prevent the condensation of the pipeline or due to temperature changes in the pipeline deformation and destruction of the wall. Dark pipe should be completed in the civil and decoration after the completion of the second system test pressure, ruled out due to civil or decorative damage caused by the pipeline, after acceptance can be put into use.

Indoor installation of PPR pipe, should be carried out after the completion of the civil decoration, with the installation of the soil before the correct hole or embedded casing. Pipeline through the floor should be set when the steel casing, casing specifications should be larger than the PPR diameter two, 50mm above the ground. PPR pipe wall should be set when the steel casing, both ends and the wall level.

埋設PPRパイプ。最後の溝の端の溝の後に溝の溝を改ざんする必要があります。硬い材料がある場合は、100 mmの厚さの砂のクッションの端に溝に敷設する必要があります。 、敷設パイプの完成後。金属管継手の埋設管など、管継手は防錆処理をしてください。パイプライン敷設は、埋め戻し前に認定されたGB50242-2002標準水圧試験に従って実施する必要があります。トレンチ埋め戻し、パイプの両側のパイプ、および砂の使用の範囲内で直径200mm以内の上部200mmの硬いものは埋め戻して含まれず、やさしくタンパーされた後、柔らかい上部の直径30mm以下土壌埋め戻しステップバイステップ。

Such as easy to find and repair the pipeline, with the PPR Pipes at the same time laying a pipe with anti-corrosion wire (available rubber metal wire), so that after the metal pipe detector to facilitate the use of metal pipe detector to determine the location of PPR pipe, easy maintenance. Buried laying PPR pipes should be below the depth of the local permafrost. Through the road or structure, should be added steel casing, casing length or width of the structure plus 1m, casing diameter should be larger than the PPR pipe diameter two.

PPR pipe has a lot of metal pipes do not have the characteristics, it is corrosion-resistant, non-scaling, smooth pipe wall, effectively prevent the water in the pipeline in the secondary pollution, and beautiful. Construction convenience, speed up the construction speed. PPR Pipes long life, can reach five times the life of galvanized pipe, basically up to the maintenance-free, greatly reducing the maintenance of operating costs. Therefore, PPR pipe in the future water supply project will be more widely used.

For PPR pipe installation, we can not be so professional, but understand the most basic welding steps can help us better check whether the installation of water pipes in line with the norms, so that the safe use of water pipes can be guaranteed.

1, the surface of the pipe and joints to ensure clean, smooth, no oil.

2, need to mark in the pipeline to try to insert. (Equal to the fitting depth of the joint).

3、パイプやジョイントを含む加熱の深さを実行するために埋め込まれた全体は、溶接ツールで実行されます。

4, to complete the heating time, the pipeline smoothly and evenly pushed into the joints, so that their combination of solid and perfect.

5, in the pipe joint welding within a few seconds, you can adjust the connector position.

6, in a short period of time, the connector can be with the load.

7, with a self-adjusting hot-melt welding machine to pipe and pipe welded together, the temperature is 260 ° C.

図8に示すように、マシンは電源(220V)に接続され、溶接温度に達している緑色の光の点滅が動作し始めたとき、しばらく待ちます。

9, because the material is light, flexible, all welding can be carried out on the table, this advantage can save man-hours.

10, sometimes in the wall to make some connections, we should pay attention to the joint location in the operating space, you can operate. If the ambient temperature is below 5 ° C, the heating time is increased by 50%.